Arlington Vagina!
Since those toy parts were probably made offshore there's a good chance they contain lead. Melt in a well ventilated area.
The silicon sealer they have in autoparts stores is good for 500 degrees and the Hi-Temp is 650 degrees. Your pewter should melt around 400 degrees, a little lower if it has lead.